Okay, here are my first results from last night.
These are 10mm test cubes. The leftmost 2 are 0.6mm layer height, and 60% infill (if I remember correctly). The one on the right is 0.4mm layer height, and 100% infill (solid).
No other changes. I'm still working out exactly what might be going on, but I think I have both temperature and cooling issues.
Advice and recommendations appreciated.
Thanks!
Stan